H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A thermal conductivity over 200 W/m K is producible.Range of Application: Switching contacts for high-voltage and medium-voltage, heat sinks for passive thermal management, electrodes for erosive processing.Information provided by H.C. Starck.
Physical Properties Metric English Comments
Density 9.80 - 10.2 g/cc
0.354 - 0.368 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 140 - 180

@Load 62.5 kg
140 - 180

@Load 138 lb
2.5 mm ball
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
Modulus of Elasticity 230 GPa
33400 ksi
Thermal Properties Metric English Comments
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 100 °C
3.44 µin/in-°F

@Temperature 68.0 - 212 °F
6.30 µm/m-°C

@Temperature 20.0 - 300 °C
3.50 µin/in-°F

@Temperature 68.0 - 572 °F
6.50 µm/m-°C

@Temperature 20.0 - 450 °C
3.61 µin/in-°F

@Temperature 68.0 - 842 °F
Thermal Conductivity >= 160 W/m-K
>= 1110 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 13 - 17 %
13 - 17 %
Molybdenum, Mo 83 - 87 %
83 - 87 %
Electrical Properties Metric English Comments
Volume Resistivity 0.0000042 ohm-cm
0.0000042 ohm-cm