Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 87.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG94 ABS (Europe-Africa-Middle East)
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Transverse to Flow 87.0 - 98.0 µm/m-°C
48.3 - 54.4 µin/in-°F
Average value: 93.7 µm/m-°C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 20.0 °C
48.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical NS-161 ABS, Antistatic, High Strength
Information Provided by LG Chem
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 20.0 °C
48.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical RS-650 ABS, Extrusion, General Purpose
Information Provided by LG Chem
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-3
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS
LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East)
LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66
LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66
LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East)
LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE
LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE)
LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 87.0 µm/m-°C
48.3 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
CTE, linear, Transverse to Flow 87.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 87.0 µm/m-°C
48.3 µin/in-°F
z, below Tg; IPC TM-650 2.4.24
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg
49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te..
Copyright © lookpolymers.com All Rights Reserved