Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East)
PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
38.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East)
Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron GR630 is a 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineering..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Colorcomp DX98735 PC
LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC
LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC
LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 69.0 - 90.0 µm/m-°C
38.3 - 50.0 µin/in-°F
Average value: 75.1 µm/m-°C Grade Count:7
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs...
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS
LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s).
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC
LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
38.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release...
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific)
This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications.
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac
RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC
LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC
LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Toyobo TS301 PPS, 30% Glass Fiber Reinforced
Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
38.3 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
CTE, linear, Transverse to Flow 69.0 µm/m-°C
38.3 µin/in-°F
ISO 11359-2
Celanese ZENITE ZE55801 LCP, 30% Specialty
Zenite« ZE55801 is a 30% glass fiber reinforced and lubricated liquid crystal polymer for injection molding and It is specifically suitable for electroless plating.Information provided by Celanese ..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba..
CTE, linear, Transverse to Flow 69.0 µm/m-°C
38.3 µin/in-°F
TMA
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound
High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo..
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 3300S Mineral Filled Novolac Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, flame retardant, novolac hardened epoxy molding compound designed to provide hermeticity protection exceeding that ..