Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 123 µm/m-°C @Temperature 23.0 - 55.0 °C |
68.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
CTE, linear, Transverse to Flow | 123 µm/m-°C @Temperature -30.0 - 30.0 °C |
68.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 123 µm/m-°C @Temperature 23.0 - 60.0 °C |
68.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WP004 is a compound based on Polybutylene Terephalate resin containing PTFE, Silicone. Added features include ; Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 123 µm/m-°C @Temperature -30.0 - 30.0 °C |
68.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 123 µm/m-°C @Temperature 23.0 - 60.0 °C |
68.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |