Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* WP004 is a compound based on Polybutylene Terephalate resin containing PTFE, Silicone. Added features include ; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
5 mm/min; ISO 527
Elongation at Yield >= 20 %
>= 20 %
5 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 132 µm/m-°C

@Temperature 23.0 - 60.0 °C
73.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 123 µm/m-°C

@Temperature 23.0 - 60.0 °C
68.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 170 °C
338 °F
Rate B/120; ISO 306
218 °C
424 °F
Rate A/120; ISO 306