Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 20.0 °C
6.67 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP130 Glass Fabric
Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP325 Cotton Fabric
Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500".
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP344 Cotton Fabric
Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining ..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP843 Paper Base Laminate
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-26B Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-28A Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-28B Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-30A Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-30B Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-28H Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-32 Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Temperature 23.0 °C
6.67 µin/in-°F

@Temperature 73.4 °F
Alliance S-26H Samarium Cobalt Magnetic Material
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
CTE, linear, Transverse to Flow 12.0 - 93.0 µm/m-°C
6.67 - 51.7 µin/in-°F
Average value: 72.3 µm/m-°C Grade Count:7
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..