Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP322 Cotton Fabric Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP325 Cotton Fabric Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500". |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP344 Cotton Fabric Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining .. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
6.67 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP843 Paper Base Laminate Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-26B Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-30B Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-28H Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-32 Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-26H Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.67 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
CTE, linear, Transverse to Flow | 12.0 - 93.0 µm/m-°C | 6.67 - 51.7 µin/in-°F | Average value: 72.3 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |