Industrial Laminates/Norplex NP843 Paper Base Laminate

Category Polymer , Thermoset , Phenolic
Manufacturer Industrial Laminates/Norplex
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex NP843 Paper Base Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through and on the surfaces.Thickness Tested: 0.062", 0.125", and 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.45 g/cc

@Thickness 1.57 mm
1.35 - 1.45 g/cc

@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 2.3 %

@Thickness 1.57 mm
2.3 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90 - 110

@Thickness 1.57 mm
90 - 110

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D638
152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity 10.0 GPa

@Thickness 1.57 mm
1450 ksi

@Thickness 0.0620 in
CW; ASTM D229
14.5 GPa

@Thickness 1.57 mm
2100 ksi

@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength 145 MPa

@Thickness 1.57 mm
21000 psi

@Thickness 0.0620 in
CW; ASTM D790
172 MPa

@Thickness 1.57 mm
25000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 303 MPa

@Thickness 12.7 mm
44000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 79.3 MPa

@Thickness 15.7 mm
11500 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.267 J/cm

@Thickness 12.7 mm
0.500 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
5.56 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 12.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
6.67 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 125 °C
257 °F
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0620 in
Descriptive Properties Value Comments
Bond Strength 1000 lb
0.5", ASTM D229
Color Black
Copyright © lookpolymers.com All Rights Reserved