Thermal Properties Metric English Comments
Glass Transition Temp, Tg 33.0 °C
91.4 °F
DSC; ASTM E1356-03
NeXolve Essar™ Stretch 255 Polyimide
High temperature colorless elastic polyimide. NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single ..
Glass Transition Temp, Tg 33.0 - 180 °C
91.4 - 356 °F
Average value: 118 °C Grade Count:40
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Glass Transition Temp, Tg 33.0 °C
91.4 °F
10°C/min; ISO 11357
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC)
TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo..
Glass Transition Temp, Tg 33.0 °C
91.4 °F
Ultimate Tg
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound
TRA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compon..
Glass Transition Temp, Tg 33.0 °C
91.4 °F
onset
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Glass Transition Temp, Tg 33.0 °C
91.4 °F
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Glass Transition Temp, Tg 33.0 °C
91.4 °F
onset
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Glass Transition Temp, Tg 33.0 °C
91.4 °F
Atom Adhesives AA-BOND 2156 Epoxy Adhesive
AA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compone..