NeXolve Essar™ Stretch 255 Polyimide

Category Polymer , Film , Thermoset , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer NeXolve Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NeXolve Essar™ Stretch 255 Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temperature colorless elastic polyimide. NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single polyimide elastomer. Essar™ Stretch 255 is a colorless polyimide elastomer with a wide variety of uses in display applications, space structures, thermal insulation, electrical insulators, industrial tapes and advanced composites. For applications requiring transparency, traditional polyimides are highly absorptive in the UV and blue region, and absorb significant amounts of energy, leading to high thermal loads.Essar Stretch™ 255 provides high optical clarity in combination with elastomer compliance. Essar™ Stretch 255 is solvent soluble and forms a tough, conformal coating upon cure. Essar™ Stretch 255 is provided as a film in continuous rolls, or as a liquid resin for spray or flow casting operations.Information Provided by NeXolve Corporation.
Mechanical Properties Metric English Comments
Tensile Strength 19.0 MPa

@Thickness 0.0500 mm
2760 psi

@Thickness 0.00197 in
ASTM D882-02
Elongation at Break 80 %

@Thickness 0.0500 mm
80 %

@Thickness 0.00197 in
ASTM D882-02
Tensile Modulus 0.0410 GPa

@Thickness 0.0500 mm
5.95 ksi

@Thickness 0.00197 in
ASTM D882-02
Thermal Properties Metric English Comments
CTE, linear 220 µm/m-°C

@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
122 µin/in-°F

@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
Glass Transition Temp, Tg 33.0 °C
91.4 °F
DSC; ASTM E1356-03
Optical Properties Metric English Comments
Refractive Index 1.49

@Wavelength 549 nm
1.49

@Wavelength 549 nm
Abbe; ASTM D542-00
UV Transmittance 50 %

@Thickness 0.0500 mm,
Wavelength 392 nm
50 %

@Thickness 0.00197 in,
Wavelength 392 nm
50% Transmission UV Cutoff
Descriptive Properties Value Comments
Applications Advanced Composites
Conformal Encapsulants
Display Applications
Electrical Insulators
Industrial Tapes
Space Structures
Thermal Insulation
Characteristics Forms a tough conformal coating
High heat stability
High optical clarity, low visible light absorption
Highly elastic, greater than 100% recoverable elastic strain
Low temperature curing
Solvent soluble
Solar Absorptivity 0.1
2 mil thickness; ASTM E903-96