Thermal Properties Metric English Comments
Glass Transition Temp, Tg 33.0 - 180 °C
91.4 - 356 °F
Average value: 118 °C Grade Count:40
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..