Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 1.84 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.84 - 2.30 J/g-°C
0.440 - 0.550 BTU/lb-°F
Average value: 1.87 J/g-°C Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Specific Heat Capacity 1.84 J/g-°C
0.440 BTU/lb-°F
Hippe PE 1000 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Specific Heat Capacity 1.84 J/g-°C
0.440 BTU/lb-°F
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Copyright © lookpolymers.com All Rights Reserved