Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 20.0 - 100 °C |
0.215 BTU/lb-°F @Temperature 68.0 - 212 °F |
Average |
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 975 Alumina, 99.5% 975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d.. |