Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | Silicone Property; ASTM E1461-01 |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 20.0 - 100 °C |
0.215 BTU/lb-°F @Temperature 68.0 - 212 °F |
DINV ENV 821-3 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 20.0 - 100 °C |
0.215 BTU/lb-°F @Temperature 68.0 - 212 °F |
Average |
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |