Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |