Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 516 - 738 °C | 961 - 1360 °F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Melting Point | 516 - 738 °C | 961 - 1360 °F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Melting Point | 516 - 560 °C | 960 - 1040 °F | |
Lucas-Milhaupt AL 719 Aluminum Brazing Filler Metal Applications:AL 719 filler metal is generally used to join aluminum and aluminum alloys. It has been used to join castings and otherwise unbrazeable aluminums. Care must be taken to be sure that t.. |
|||
Melting Point | 516 °C | 960 °F | |
Heatbath/Park Alu-Braze 960 Aluminum Brazing Salt This is the standard salt designed for low melting point, good fluidity, and good braze characteristics.Information provided by Heatbath Corporation - Park Metallurgical. |