Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 516 - 738 °C | 961 - 1360 °F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Melting Point | 516 - 738 °C | 961 - 1360 °F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |