Material Notes:
Applications:AL 719 filler metal is generally used to join aluminum and aluminum alloys. It has been used to join castings and otherwise unbrazeable aluminums. Care must be taken to be sure that the heat treatment (if any) is compatible with the brazing materials and process. Because of this high alloy content of AL 719, the corrosion resistance is not as good as other aluminum filler metals. Characteristics:AL 719 is a filler metal for use with brazeable aluminums where a flux process is used. Because of its high zinc content this material is not recommended for vacuum brazing. To prevent liquation, it is recommended that the parts be heated rapidly thru the solidus-liquidus temperature range. Specifications: AL 719 meets the requirements for the following specifications-Aluminum Association (AA) 4245 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 2.91 g/cc
0.105 lb/in³
Thermal Properties Metric English Comments
Melting Point 516 - 560 °C
960 - 1040 °F
Solidus 516 °C
960 °F
Melting Point
Liquidus 560 °C
1040 °F
Flow Point
Component Elements Properties Metric English Comments
Aluminum, Al >= 72.74 %
>= 72.74 %
Chromium, Cr <= 0.070 %
<= 0.070 %
Copper, Cu 3.3 - 4.7 %
3.3 - 4.7 %
Iron, Fe <= 0.80 %
<= 0.80 %
Magnesium, Mg <= 0.070 %
<= 0.070 %
Manganese, Mn <= 0.070 %
<= 0.070 %
Other, each <= 0.050 %
<= 0.050 %
Other, total 0.15 %
0.15 %
Silicon, Si 9.3 - 10.7 %
9.3 - 10.7 %
Zinc, Zn 9.3 - 10.7 %
9.3 - 10.7 %
Processing Properties Metric English Comments
Processing Temperature 549 - 571 °C
1020 - 1060 °F
Brazing Range
Descriptive Properties Value Comments
Color Grayish-White