Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2500 °C | 4530 °F | |
MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
Melting Point | 2500 °C | 4530 °F | |
H.C. Starck Baymetec® Tantalum Silicide, Ta5Si3 Baymetec® Silicides are highly purity powders manufactured for exacting semiconductor and electronic applications.Gate metal for high-k dielectricsSemiconductorsElectrode for SiC high power semic.. |
|||
Melting Point | 2500 - 2600 °C | 4530 - 4710 °F | |
Goodfellow TZM Molybdenum High Temperature Alloy Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow. |
|||
Melting Point | 2500 °C | 4530 °F | |
Mateck YSZ Substrate bicrystals for superconductivity |