Thermal Properties Metric English Comments
Melting Point 2500 - 2600 °C
4530 - 4710 °F
Goodfellow TZM Molybdenum High Temperature Alloy
Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow.