MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
Physical Properties Metric English Comments
Density 5.80 g/cc
0.210 lb/in³
a Lattice Constant 5.41 Ã…
5.41 Ã…
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 °C
5.72 µin/in-°F

@Temperature 68.0 °F
Melting Point 2500 °C
4530 °F
Electrical Properties Metric English Comments
Dielectric Constant 27
27