Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2500 - 2600 °C | 4530 - 4710 °F | |
Goodfellow TZM Molybdenum High Temperature Alloy Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow. |