Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 300 - 314 °C | 572 - 597 °F | |
Williams Advanced Alloys WS314 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 310 - 314 °C | 590 - 597 °F | |
Williams Advanced Alloys WS314A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |