Thermal Properties Metric English Comments
Melting Point 1600 °C
2910 °F
Reade Advanced Materials Strontium Sulfate Powder (Celestite) (SrSO4)
Description: A mineral source of strontium and its compounds. Sometimes used to impart iridescence to glass and pottery glazes. Used as a fining agent in crystal glass.Information provided by Reade..
Melting Point 1600 °C
2910 °F
MarkeTech Lithium Gallium Oxide (LiGaO2) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 0.2%.
Melting Point 1600 °C
2910 °F
MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.2%.
Melting Point 1600 °C
2910 °F
Mateck Barium Titanate Crystal, BaTiO3
Oxidic single crystals. Two-wave mixing coupling constant. BaTiO3 is a very unique crystal with superior photo-refractive and ferroelectric properties. MaTecK supplies both of substrate grade and ph..
Melting Point 1600 °C
2910 °F
Mateck LiGaO2
Substrate single crystals for III-V nitrides
Melting Point 1600 °C
2910 °F
Mateck Neodymium Gallate Substrate, NdGaO3
Substrate single crystals for superconductivity
Melting Point 1600 °C
2910 °F
Mateck SrLaGaO4
Substrate single crystals for superconductivity
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Annealed Bar 0.5 - 1.23 in. dia
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Solution Treated Annealed Bar 0.5 - 1.23 in. dia
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded, Mill Annealed
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 - 1650 °C
2910 - 3000 °F
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Melting Point 1600 °C
2910 °F
Goodfellow Titanium 78/Aluminum 22 Alloy
Information provided by Goodfellow.