Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1600 °C
2910 °F
Component Elements Properties Metric English Comments
Aluminum, Al 22 %
22 %
Titanium, Ti 78 %
78 %