Reade Advanced Materials Strontium Sulfate Powder (Celestite) (SrSO4)

Category Ceramic
Manufacturer Reade Advanced Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reade Advanced Materials Strontium Sulfate Powder (Celestite) (SrSO4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A mineral source of strontium and its compounds. Sometimes used to impart iridescence to glass and pottery glazes. Used as a fining agent in crystal glass.Information provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 3.80 - 4.00 g/cc
3.80 - 4.00 g/cc
Bulk Density 3.96 g/cc
0.143 lb/in³
Molecular Weight 183.682 g/mol
183.682 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 3.0 - 3.5
3.0 - 3.5
Thermal Properties Metric English Comments
Melting Point 1600 °C
2910 °F
Descriptive Properties Value Comments
Color white