Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 141 °C | 286 °F | HS Method |
Hyosung Topilene R200P PP R200P Extrusion Random CopolymerApplications:Underfloor heating pipeWater service pipeCharacteristics:Pressure resistanceHigh impactLong-term heat stabilityFlexibilityInformation provided by Hyosung.. |
|||
Melting Point | 141 °C | 286 °F | DSC |
Shakespeare Isocorâ„¢ TT52SI Nylon 6 Terpolymer Isocorâ„¢ TT52SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ TT52SI is easily processed and has a wide range of application.. |
|||
Melting Point | 141 - 144 °C | 286 - 291 °F | ISO 416C |
Shanghai Ofluorine 9201F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Melting Point | 141 - 144 °C | 286 - 291 °F | ISO 416C |
Shanghai Ofluorine 9202F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Melting Point | 141 °C | 286 °F | DSC; ISO 3146 |
Borealis Bormed™ SC820CF Polypropylene Random Copolymer Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist.. |
|||
Melting Point | 141 - 144 °C | 286 - 291 °F | ISO 416C |
Shanghai Ofluorine 9201 PVDF Pellets for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |