Material Notes:
R200P Extrusion Random CopolymerApplications:Underfloor heating pipeWater service pipeCharacteristics:Pressure resistanceHigh impactLong-term heat stabilityFlexibilityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 0.20 g/10 min
0.20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 0.834 GPa
121 ksi
ASTM D790
Izod Impact, Unnotched NB
NB
ASTM D256
0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 141 °C
286 °F
HS Method
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525