Borealis Bormed™ SC820CF Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ SC820CF Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antistatic additives or nucleating additivesInformation provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 0.330 GPa
47.9 ksi
MD/TD; ISO 527-3
Flexural Modulus 0.550 GPa
79.8 ksi
50% humidity; ISO 178
Dart Drop, Total Energy 15.0 J
11.1 ft-lb
1200N; ISO 7765-2
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ISO 527-3
Film Tensile Strength at Break, TD 50.0 MPa
7250 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 141 °C
286 °F
DSC; ISO 3146
Vicat Softening Point 120 °C

@Load 1.02 kg
248 °F

@Load 2.25 lb
A50; ISO 306
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Gloss >= 120 %
>= 120 %
20° of arc; ASTM D2457