Shanghai Ofluorine 9202F PVDF Powder for cables

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Shanghai Ofluorine
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shanghai Ofluorine 9202F PVDF Powder for cables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, low fog, low flame spread characteristics.Information provided by Shanghai Ofluorine Chemical Technology
Physical Properties Metric English Comments
Specific Gravity 1.77 - 1.78 g/cc
1.77 - 1.78 g/cc
ISO R1183D
Particle Size <= 30 µm
<= 30 µm
Average size before sieving
Melt Flow 2.0 - 6.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
2.0 - 6.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ISO 868
Tensile Strength at Break >= 26.0 MPa

@Strain >=100 %
>= 3770 psi

@Strain >=100 %
ISO R527
Elongation at Break >= 100 %
>= 100 %
ISO R527
Flexural Strength 680 MPa
98600 psi
ISO 178
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Melting Point 141 - 144 °C
286 - 291 °F
ISO 416C
Heat Distortion Temperature 48.0 °C
118 °F
ISO 75
Oxygen Index 43 %
43 %
ASTM D2863