Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® M90AW POM, Tribological  (Unverified Data**)
Celcon® M90AW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear in low load-high velocity applications. Celcon® M90AW is an option ..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® UV270Z POM, UV Resistant  (Unverified Data**)
Celcon® UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® C 9021 LS 10/1570 POM, UV Resistant  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMGeneral purpose injection molding grade, UV-stabilized with UV stabilzers and carbon blackInformation provided by Celanese
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® LG450UV-D POM, UV Resistant  (Unverified Data**)
Hostaform® acetal copolymer grade LG450UV-D is a specialty grade of acetal copolymer formulated to provide high flow with a reduced gloss finish and a UV stability necessary for interior automotive..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® LM25 POM, Specialty  (Unverified Data**)
Hostaform® LM25 is a 2.5 melt flow acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform® LM25 can be lasermarked with bar-codes, identification num..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® M90LF POM  (Unverified Data**)
Hostaform® acetal copolymer grade M90LF is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film.Stan..
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 GF5 POM
26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 GF6 POM
30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 GF7 POM
35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 HI2 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 500 GF6 POM
30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr..
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 700 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® GC90UV POM, 10% UV Resistant
Celcon« acetal copolymer grade GC90UV is a specialty grade combining glass coupling for improved strength and stiffness and UV stabilization for improved performance in exposure to artificial light..
Melting Point 167 °C
333 °F
ASTM Test
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.
Melting Point 167 °C
333 °F
DIN 53765
BASF Ultraform® N2320 0035 LEV POM
Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF
Melting Point 167 °C
333 °F
ISO 11357-1/-3
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Melting Point 167 °C
333 °F
DIN 53765
BASF Ultraform® S2320 0035 POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® LM25 POM, Specialty
Hostaform« LM25 is a 2.5 melt flow acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« LM25 can be lasermarked with bar-codes, identification num..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® LGC90-QX POM, 26% Glass Reinforced
Preliminary Data Sheet26% long fiber glass filled, high strengthLong Fiber Reinforced Thermoplastic products may be processed using current standard injection molding machines having screw diameters..
Melting Point 167 °C
333 °F
DSC
Arkema Group OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene
OREVAC® CA 100 is a chemically functionalized polypropylene with a high content of maleic anhydride. Grafting on polypropylene backbone is achieved with a processing technology which allows to opti..
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 GB4 POM
20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 300 HI6 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melting Point 167 °C
333 °F
BASF Ultraform® S2320 003 PRO BK 00120 POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® CF802 POM, Specialty  (Unverified Data**)
Celcon® acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon® CF802 has been developed to dissipate static electricity from fuel handling systems...
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® LM90Z POM, Specialty  (Unverified Data**)
Celcon® LM90Z is a UV stable, nominal 9 melt flow acetal copolymer which is capable of being permanently marked by a laser. It gives protection against property and color deterioration in applicati..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celcon® M90-45XAP® POM, Specialty  (Unverified Data**)
Celcon® acetal copolymer grade M90-45XAP® is a UV resistant, low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the in..
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® M10AE POM  (Unverified Data**)
POM copolymerHigh melt strengthInformation provided by Celanese
Melting Point 167 °C
333 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Hostaform® M90XAP® POM  (Unverified Data**)
Hostaform® acetal copolymer grade M90 XAP® is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo..
Melting Point 167 °C
333 °F
DSC
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..