Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1370 - 1430 °C | 2500 - 2610 °F | |
Pyramid Stainless Steel AISI 304/316L, STAINLESS STEEL SHEET NO.4 FINISH Information provided by Pyramid Stainless Steel Ind Co Ltd |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Melting Point | 1370 - 1430 °C | 2500 - 2610 °F | |
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy Data provided by the manufacturer, Special Metals. |
|||
Melting Point | 1370 - 1400 °C | 2500 - 2550 °F | |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Melting Point | 1370 - 1400 °C | 2500 - 2550 °F | |
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |
|||
Melting Point | 1370 - 1400 °C | 2500 - 2550 °F | |
Crucible Steel 347 Chromium-Nickel Steel Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Melting Point | 1370 - 1400 °C | 2500 - 2550 °F | |
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Melting Point | 1370 - 1510 °C | 2500 - 2750 °F | |
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
Melting Point | 1370 - 1510 °C | 2500 - 2750 °F | |
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
Melting Point | 1370 - 1480 °C | 2500 - 2700 °F | |
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
Melting Point | 1370 °C | 2500 °F | |
California Fine Wire Permanickel® K-300 Nickel Alloy All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif.. |
|||
Melting Point | 1370 - 1400 °C | 2500 - 2550 °F | |
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Melting Point | 1371 - 1399 °C | 2500 - 2550 °F | |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Melting Point | 1371 - 1399 °C | 2500 - 2550 °F | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Melting Point | 1370 °C | 2500 °F | |
Alloy Wire International RW 118 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Melting Point | 1371 - 1399 °C | 2500 - 2550 °F | |
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |
|||
Melting Point | 1370 - 1430 °C | 2500 - 2610 °F | |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Melting Point | 1370 - 1418 °C | 2500 - 2584 °F | |
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
Melting Point | 1370 - 1520 °C | 2500 - 2770 °F | |
Johnson Matthey HS Platinum Jewelry Alloy Hard springy, can be cast for catches. |