Polymer Property : Melting Point = 1250 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 675 - 735 °C
1250 - 1360 °F
Johnson Matthey Matti-sil 45 Cadmium Free Brazing Alloy
A medium flowing alloy which is often used for marine and Shipbuilding applications.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-5BS EN 1044 1999 AG203Federal Specification QQ-B-564 BAg-5Equival..
Melting Point 677 - 857.2 °C
1250 - 1575 °F
Lucas-Milhaupt BRAZE 250 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 250 is an intermediate temperature silver brazing alloy with a long (325EF/180EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constitu..
Melting Point 677 - 766 °C
1250 - 1410 °F
Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 300 is an intermediate temperature silver brazing alloy with a fairly long (160EF/70EC) melting range. This long melting range is helpful when wide gap joints are brazed and ..
Melting Point 677 - 766 °C
1250 - 1410 °F
Lucas-Milhaupt Silvaloy® A30 Brazing Alloy
Silvaloy A30 does not contain cadmium and is often used as an alternate to cadmium containing alloys when the brazed assembly comes in contact with food or dairy products. Its slightly higher melt t..
Melting Point 677 - 773.9 °C
1250 - 1425 °F
Lucas-Milhaupt Silvaloy® A50 Brazing Alloy
Silvaloy A50 is widely used for brazing in the electrical industry, as well as in the dairy and food industries where the use of cadmium-containing filler metals is prohibited. Silvaloy A50 has a br..
Melting Point 675 - 765 °C
1250 - 1410 °F
Johnson Matthey Matti-sil 30 Cadmium Free Brazing Alloy
The wide melting range of Matti-sil 30 makes it suitable for filling larger joint gaps and producing fillets where desired.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-20Federal Specification QQ..