Lucas-Milhaupt Silvaloy® A50 Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® A50 Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy A50 is widely used for brazing in the electrical industry, as well as in the dairy and food industries where the use of cadmium-containing filler metals is prohibited. Silvaloy A50 has a broad melting range making it a good choice for filler wide joint clearances or forming large fillets.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Thermal Properties Metric English Comments
Melting Point 677 - 773.9 °C
1250 - 1425 °F
Solidus 677 °C
1250 °F
Liquidus 773.9 °C
1425 °F
Component Elements Properties Metric English Comments
Copper, Cu 33 - 35 %
33 - 35 %
Silver, Ag 49 - 51 %
49 - 51 %
Zinc, Zn 14 - 16 %
14 - 16 %
Processing Properties Metric English Comments
Processing Temperature 743 - 843 °C
1370 - 1550 °F
Brazing Temperature