Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 603 - 705 °C | 1120 - 1300 °F | |
Indium Corp. Indalloy 179 Silver Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 605 - 710 °C | 1120 - 1310 °F | |
Indium Corp. Indalloy 212 Ag-Cu-Zn-Cd Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 605 - 620 °C | 1120 - 1150 °F | |
Indium Corp. Indalloy 215 Silver Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 605 - 745 °C | 1120 - 1370 °F | |
Johnson Matthey Mattibraze 30 Cadmium Containing Silver Brazing Alloy An economic alternative with a wider melting range ideal for a gap filler.Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. The l.. |
|||
Melting Point | 605 - 700 °C | 1120 - 1290 °F | |
Johnson Matthey Mattibraze 35 Cadmium Containing Silver Brazing Alloy A free flowing alloy suitable for larger joint clearances and forming fillets.Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. T.. |
|||
Melting Point | 605 - 620 °C | 1120 - 1150 °F | |
Johnson Matthey Mattibraze 45 Cadmium Containing Silver Brazing Alloy Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. The localized extraction of fumes during brazing is now virtually obligatory. .. |
|||
Melting Point | 602 - 718 °C | 1120 - 1320 °F | |
Williams Advanced Alloys Wambraze™ WB718 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Melting Point | 604 - 729.4 °C | 1120 - 1345 °F | |
Lucas-Milhaupt BRAZE 580 Silver Based Cadmium Free Filler Metal Characteristics:Braze 580 is a free flowing intermediate temperature cadmium-free silver brazing filler metal that exhibits an unusual ability to wet certain base metals that are difficult to braze .. |
|||
Melting Point | 605 - 700 °C | 1120 - 1290 °F | |
Indium Corp. Indalloy 219 Ag-Au-Zn-Cd Solder Alloy Information Provided by Indium Corporation |