Indium Corp. Indalloy 215 Silver Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 215 Silver Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.11 g/cc
0.329 lb/in³
Thermal Properties Metric English Comments
Melting Point 605 - 620 °C
1120 - 1150 °F
Solidus 605 °C
1120 °F
Liquidus 620 °C
1150 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 24 %
24 %
Copper, Cu 15 %
15 %
Silver, Ag 45 %
45 %
Zinc, Zn 16 %
16 %