Johnson Matthey Mattibraze 30 Cadmium Containing Silver Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Mattibraze 30 Cadmium Containing Silver Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An economic alternative with a wider melting range ideal for a gap filler.Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. The localized extraction of fumes during brazing is now virtually obligatory. The use of cadmium containing alloys is not permitted in the manufacture of food and drink handling equipment and medical instruments. If cadmium containing alloys are felt likely to cause a health hazard then use a cadmium free alloy from the Johnson Matthey Matti-sil range. Full details on exposure levels (OES) are given in the specific Material Safety Data Sheets. These should always be consulted before use of a cadmium bearing brazing alloy.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-2aEquivalent to Engelhard Silvaloy 30Equivalent to Handy & Harman Easy-flo 30Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 605 - 745 °C
1120 - 1370 °F
Solidus 605 °C
1120 °F
Liquidus 745 °C
1370 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 20 %
20 %
Copper, Cu 27 %
27 %
Silver, Ag 30 %
30 %
Zinc, Zn 23 %
23 %