Lucas-Milhaupt BRAZE 580 Silver Based Cadmium Free Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name BRAZE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt BRAZE 580 Silver Based Cadmium Free Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Braze 580 is a free flowing intermediate temperature cadmium-free silver brazing filler metal that exhibits an unusual ability to wet certain base metals that are difficult to braze with more standard alloys. Typical of these base metals are chromium and tungsten carbides. Unlike some other manganese containing brazing filler metals, Braze 580 does not tend to produce porous fillets. Braze 580 contains no zinc or cadmium and will not outgas during Titanium Nitride coating of tools. Applications:This alloy should be regarded as a special purpose material for brazing difficult to wet metals and alloys such as tungsten and chromium carbides. Wetting studies show that this alloy exhibits excellent wetting in vacuum brazing of high manganese stainless steels. For details consult: Vacuum Brazing of High Manganese Stainless Steel by W. S. Bennett and R.F. Hillyer, Welding Journal (Vol 53, No. 11, Nov. 1974, P510S).Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.82 g/cc
0.355 lb/in³
Thermal Properties Metric English Comments
Melting Point 604 - 729.4 °C
1120 - 1345 °F
Solidus 604 °C
1120 °F
Melting Point
Liquidus 729.4 °C
1345 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu 31.5 - 33.5 %
31.5 - 33.5 %
Manganese, Mn 2.5 - 3.5 %
2.5 - 3.5 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 56.5 - 58.5 %
56.5 - 58.5 %
Tin, Sn 6.5 - 7.5 %
6.5 - 7.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000681 ohm-cm
0.00000681 ohm-cm
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: