Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 107 °C | 225 °F | Internal method |
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti.. |
|||
Melting Point | 107 °C | 225 °F | Internal method |
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i.. |
|||
Melting Point | 107 °C | 225 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Melting Point | 107 °C | 225 °F | Exxon Method |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Melting Point | 107 °C | 225 °F | 10°C/min; DSC |
LG Chemical LUTENE LB4500 LDPE Extrusion Coating Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silico.. |
|||
Melting Point | 107 °C | 225 °F | 10°C/min; DSC |
LG Chemical LUTENE LB5000 LDPE Extrusion Coating Description: LUTENE LB5000 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB5000 is also noted for the excellent adhesion to porous a.. |
|||
Melting Point | 107 °C | 225 °F | 10°C/min; DSC |
LG Chemical LUTENE LB7500 LDPE Extrusion Coating Description: LUTENE LB7500 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB7500 is also noted for the excellent adhesion to porous a.. |
|||
Melting Point | 107 °C | 225 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC BF410 LDPE Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG .. |
|||
Melting Point | 107 °C | 225 °F | Kofler; SRTM 3022-9 |
Lubrizol Estane® UB400 Thermoplastic Polyurethane Type: Estane® UB400 is a Shore 78A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in AsiaI.. |
|||
Melting Point | 107 °C | 225 °F | ASTM D-3418 |
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi.. |
|||
Melting Point | 107 °C | 225 °F | ASTM D3418, ISO 3146 |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |
|||
Melting Point | 107 °C | 225 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Melting Point | 107 °C | 225 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
Melting Point | 107 °C | 224 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Melting Point | 107 °C | 225 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Melting Point | 107 °C | 225 °F | Dow Method (DSC) |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |
|||
Melting Point | 107 °C | 224 °F | Dow Method (DSC) |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Melting Point | 107 °C | 225 °F | DSC |
Arkema Group LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate LOTRYL® 7 BA 01 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 7 BA 01 is used for film coextrusion and lamination where sealab.. |
|||
Melting Point | 107 - 111 °C | 225 - 232 °F | |
BASF Piperazine Chips Formula: C4H10N2CAS: 110-85-0Description: Piperazine chips is a colorless to yellow solid with an amine-like odor. The hygroscopic crystalline chips are soluble in water, methanol, and ethanol Syno.. |
|||
Melting Point | 107 °C | 225 °F | DSC |
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline .. |
|||
Melting Point | 107 °C | 225 °F | DSC |
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi.. |