Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 20.0 °C
45.6 µin/in-°F

@Temperature 68.0 °F
Eastman Eastar DN101 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
CTE, linear, Parallel to Flow 82.0 µm/m-°C
45.6 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber
PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic..
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
45.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12
LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 20.0 °C
45.6 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ HPC 952 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MK0049A PP (Europe-Africa-Middle East)
LNP* STARFLAM* MK0049A is a compound based on Polypropylene resin containing Talc, Flame Retardant. Added features include : Flame Retardant.
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East)
Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 20.0 °C
45.6 µin/in-°F

@Temperature 68.0 °F
Ineos ABS NOVODUR® P2T ABS, Injection Grade  (discontinued **)
Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g..