Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 20.0 °C |
45.6 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
45.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C | 45.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 20.0 °C |
45.6 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MK0049A PP (Europe-Africa-Middle East) LNP* STARFLAM* MK0049A is a compound based on Polypropylene resin containing Talc, Flame Retardant. Added features include : Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 20.0 °C |
45.6 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |