Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP COLORCOMP J1000AE PES LNP* COLORCOMP* J1000AE is an unfilled Polyethersulfone. Added feature of this grade is: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear (Europe-Africa-Middle East) LNP* Lubricomp* OL004 is a compound based on PPS - Linear resin containing PTFE. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU) Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630Q PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.9 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8792 Polyimide DuPont Vespel TP-8792 parts are specified for mechanical, thermal, and tribological properties. TP-8792 offers excellent strength and toughness, dimensional stability, low outgassing, radiation resi.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® S 4090 GX 14% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ISO 11359-1/-2 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded BG3ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ISO 11359-2 |
Celanese FORTRON 317 PPS, Unfilled 0317 exhibits a high melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding monofilament/fibers, r.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |