Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BG3ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Water Absorption at Saturation 5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
ISO 62-1
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
on Tensile Bar, Flow; ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
5 mm/min; ISO 527
Elongation at Break 10 %
10 %
5 mm/min; ISO 527
Tensile Modulus 4.50 GPa
653 ksi
1 mm/min; ISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -40.0 °C
3.33 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
12.0 kJ/m²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
18.0 kJ/m²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature 23.0 - 60.0 °C
56.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 550 V
550 V
IEC 60112