Polymer Property : CTE, linear, Parallel to Flow = 42.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific)
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East)
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
Eastman Eastapak 7352 PET  (discontinued **)
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
ISO data
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO
LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 100 °C
42.8 µin/in-°F

@Temperature -40.0 - 212 °F
ASTM E831
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 100 °C
42.8 µin/in-°F

@Temperature -40.0 - 212 °F
ASTM E831
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications.
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
Eastman Eastar 6763 PETG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical