Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Antistat/Conductive , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Retardant.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0042 cm/cm

@Time 86400 sec
0.0042 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
ISO 527
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Elongation at Yield 3.3 %
3.3 %
ISO 527
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
Flexural Strength 102 MPa
14800 psi
ISO 178
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 43.0 kJ/m²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D 257
Surface Resistance 1000 ohm
1000 ohm
ASTM D 257
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
Copyright © lookpolymers.com All Rights Reserved