Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-46 Adhesive, Sealant & Coating System Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.Applications: Very high flexibility, 500% elongation, emphasizing high tack for un-abraded sub.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-4682 Adhesive, Sealant & Coating System Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.Applications: High flexibility, 300% elongation, emphasizing high tack for un-abraded substrat.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-4811 Adhesive, Sealant & Coating System Key Properties: Semi-rigid, high strength.A filled version of B-481 to further increase chemical resistance and electrical properties and to lower shrinkage.Ease of use.Applications: Encapsulate sen.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-482 Adhesive, Sealant & Coating System Key Properties: Excellent balance of chemical, electrical, and mechanical properties.Ruggedized, semi-flexible system.Very clean system.Ease of use.Applications: Encapsule sensitive instrumentation .. |
|||
Minimum Service Temperature, Air | -45.6 - -17.8 °C | -50.0 - 0.000 °F | Average value: -28.9 °C Grade Count:29 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System Key Properties: High strength and toughness with excellent thermal stability to 400°F.Outstanding chemical resistance.Excellent electrical, and mechanical properties.Ease of use.Applications: Encap.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | Retraction Temperature, TR10; ASTM D1329 |
Freudenberg Simrit N432 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | Retraction Temperature, MIL-H-5606 fluid immersion for 70 hours at 275°F; ASTM D1329 |
Freudenberg Simrit N432 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | Retraction Temperature, TR10; ASTM D1329 |
Freudenberg Simrit S315 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | Approx. Cold test |
Lubriplate SYN SYN-1600 PAO-Based Multi-Purpose Grease Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | Approx. Cold test |
Lubriplate SYN SYN-1601 PAO-Based Multi-Purpose Grease Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Whitecast Polymer Engineering Epoxy Composite Casting Whitecast Polymer Engineering (WPE) low-density material is used for acoustic dampening requirements (Damping ratio = 0.158). There is an order of magnitude higher vibration dampening realized when.. |
|||
Minimum Service Temperature, Air | -45.6 °C | -50.0 °F | |
Bostik 6368 Fast Setting EVA Glue Stick Bostik 6368 Fast Setting EVA Glue StickDesigned for packaging. Good temperature resistance. Fast setting. |