Material Notes:
Key Properties: High strength and toughness with excellent thermal stability to 400°F.Outstanding chemical resistance.Excellent electrical, and mechanical properties.Ease of use.Applications: Encapsule sensitive instrumentation for chemical isolation, outstanding moisture resistance, ruggedness and flexibility. Suitable for clean room use and direct contact with semiconductors. Very easy to use and very clean two-part system. Superior for coating in marine applications and other harsh environments. Tough, high strength, chemically resistant non-blush clear coating with medium gloss finish. Bonds to most substrates. Can be applied to oily surfaces. Ambient 24 hour or accelerated thermal cure.
Physical Properties Metric English Comments
Water Absorption <= 1.0 %
<= 1.0 %
24hrs boiling DI water
Viscosity 2500 cP
2500 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.48 MPa
4566 psi
3 hrs @ 200°F; 2:1 Volume Mix
Tensile Strength, Ultimate 33.05 MPa
4794 psi
Peak; 3 hrs @ 200°F; 2:1 Volume Mix
Tensile Strength, Yield 33.05 MPa
4794 psi
3 hrs @ 200°F; 2:1 Volume Mix
Elongation at Break 12.9 %
12.9 %
3 hrs @ 200°F; 2:1 Volume Mix
Elongation at Yield 9.6 %
9.6 %
3 hrs @ 200°F; 2:1 Volume Mix
Tangent Modulus 623.46 MPa
90425 psi
3 hrs @ 200°F; 2:1 Volume Mix
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -45.6 °C
-50.0 °F
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
Ambient Set
720 min
12.0 hour
Ambient, tack free
1440 min
24.0 hour
Ambient, 95% cure
120 min

@Temperature 65.6 °C
2.00 hour

@Temperature 150 °F
98% cure
Pot Life 40 min
40 min
Ambient
Descriptive Properties Value Comments
Chemical & Moisture Resistance 3.5
0=Lowest, 4=Highest
Color Clear with slight amber