Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 72.0 °C @Load 1.00 kg |
162 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green.. |
|||
Vicat Softening Point | 72.0 °C @Load 1.00 kg |
162 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A.. |
|||
Vicat Softening Point | 72.0 °C @Load 1.00 kg |
162 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
Karina E818-10/23-CRM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
Karina E818-18/99-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | |
LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | |
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | A; ISO 306 |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
Mitsui ADMER® AT1053A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
Karina 806-48/1-BY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
Karina E 818-10/23-CRM-AS White PVC Compound UV. protection addedInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high dens.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | Rate "B" Loading 1 (120 degC/h 10N); ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | Rate "B" Loading 1 (120 degC/h 10N); ASTM Test |
Styrolution Styrolux HS 70 SBC Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Vicat Softening Point | 72.0 °C @Load 5.10 kg |
162 °F @Load 11.2 lb |
B50; ISO 306 |
Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | B (50N); ISO 306 |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
DuPont Bynel® 39E660 Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | 120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | |
BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1005 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and very high mechanical properties. Examples: high strength stretch film, greenhous.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | |
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |