Thermal Properties Metric English Comments
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & M..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene® LD 720.62 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene® LD 721.IK Film Resin
Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Ap..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame..
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b..
Copyright © lookpolymers.com All Rights Reserved