Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: CompoundingHot Melt AdhesivesInjection MoldingWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 18 %
18 %
ExxonMobil method
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89

@Time 15.0 sec
89

@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0503 GPa
7.30 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 187 °C
<= 369 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 240